E-27H15N35V3G2B2T
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Nb, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10052-75 | 37.682–47.63 | < 0.7 | 1.5–2.5 | 13.5–16 | 0.05–0.25 | 33–36.5 | < 0.018 | 0.22–0.32 | < 0.03 | 1.7–2.5 | 2.4–3.5 |
Note: Nb> 8 * C
Note: The chemical composition of the weld metal
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10052-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| W | % | Tungsten |