E-350H26G2R2ST
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10051-75 | 60.425–69.8 | 0.6–1.2 | 1.8–2.5 | 1.5–2.5 | 23–29 | 0.2–0.4 | < 0.04 | 3.1–3.9 | < 0.035 |
Note: The chemical composition of the weld metal
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10051-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |