EI13
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|
| 95.16–96.6 | 0.2–0.3 | 0.5–1.1 | 0.8–1.1 | < 0.02 | 1.1–1.2 | < 0.02 | 0.8–1.1 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.89 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |