EI200
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| 95.903–97.25 | 0.15–0.35 | 0.2–0.4 | 1.3–1.65 | < 0.2 | 0.15–0.35 | < 0.027 | 0.95–1.1 | < 0.02 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.78 g / cm3 |