CIS, Russia, Ukraine Corrosion-resistant alloys and steels Corrosion-resistant alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ni, % V, % P, % C, % S, % Mo, % W, %
91.79–92.84 0.15–0.25 0.3–0.4 1.5–1.7 3.5–3.7 0.15–0.2 < 0.02 0.36–0.42 < 0.02 0.4–0.5 0.8–1

Information on suppliers

Свойства

Свойство
Вычисляемые свойства Плотность: 7.97 г/см3