EI236 (120G13)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-1614-76 | 82.37–88 | < 0.7 | 11–14 | < 0.5 | < 0.3 | < 0.6 | < 0.1 | 1–1.4 | < 0.03 |
Note: The chemical composition may be changed by agreement.
Information on suppliers
Properties
| Property |
|---|
| According to TU 14-1-1614-76 Note Quenching Hardness HB: <217 Ink diameter:> 4.1 mm |
| Calculated Properties Density: 7.72 g / cm3 |
| Note austenitic steel Forged and hot rolled |
Standards
| Standard | Description |
|---|---|
| TU 14-1-1614-76 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |