EI247
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 94.82–96.98 | 0.17–0.37 | 0.3–0.6 | 1.35–1.65 | < 0.5 | 0.5–1 | < 0.03 | 0.3–0.4 | < 0.03 | 0.4–0.6 |
Information on suppliers
Properties
| Property |
|---|
| Calculated properties Density: 7.8 g / cm3 |