EI334 (ХН80)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ca, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
| TU 14-1-997-2012 |
< 1.7 |
< 0.6 |
< 0.5 |
0.2–1.5 |
20–23 |
< 0.25 |
< 0.07 |
71.98–79.8 |
< 0.1 |
< 0.03 |
< 0.25 |
< 0.02 |
Information on suppliers
Properties
| Property |
| According to TU 14-1-997-2012 Note Mechanical properties are not standardized Mechanical properties: as agreed |
| Calculated Properties Density: 8.43 g / cm3 |
Analogues
| Germany |
USA |
| CHRONITHERM 80 SPEZIAL |
Nichrome V |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Ca |
% |
Calcium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |