EI361
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 73.34–81 | < 1 | < 0.7 | 15–18 | 0.5–0.7 | < 0.6 | 3.5–5.5 | < 0.03 | < 0.1 | < 0.03 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.46 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |