EI377
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| 95.885–97.56 | 0.17–0.37 | 0.6–0.9 | 1.25–1.65 | < 0.5 | < 0.03 | 0.17–0.23 | < 0.035 | 0.25–0.4 |
Information on suppliers
Свойства
| Свойство |
|---|
| Вычисляемые свойства Плотность: 7.84 г/см3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |