EI382
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 84.77–88.8 | < 0.4 | < 0.4 | 4.5–5.5 | 0.1–0.3 | < 0.4 | 1.8–2.3 | 0.8–0.9 | < 0.03 | 4–5 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 8.24 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| V | % | Vanadium |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |