EI395 (St-10H16N25AM6)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU 14-1-3146-81 |
45.13–53.9 |
0.5–1 |
1–2 |
15–17.5 |
24–27 |
< 0.03 |
< 0.12 |
< 0.02 |
5.5–7 |
0.1–0.2 |
Information on suppliers
Properties
| Property |
| Calculated Properties Density: 8.11 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |