EI402ML (10H17N10G4MBL)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| OST 108.961.04-80 |
< 3 |
< 0.6 |
0.01 |
< 0.5 |
15–17 |
1.3–1.6 |
60.988–70.265 |
1.4–1.7 |
0.025 |
< 0.015 |
< 0.05 |
< 0.012 |
3.5–4.5 |
8.5–10 |
Information on suppliers
Properties
| Property |
| Castings Yield strength:> 200 MPa Tensile strength:> 400 MPa Elongation:> 15% Impact strength KCU at 20 ° C:> 40 J / cm2 Relative narrowing:> 25% |
| Calculated Properties Density: 7.85 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |