EI471
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 96.305–97.688 | 0.15–0.35 | 0.002–0.005 | 1–1.3 | 0.9–1.3 | 0.08–0.15 | < 0.3 | < 0.03 | 0.18–0.23 | < 0.03 |
Information on suppliers
Свойства
| Свойство |
|---|
| Вычисляемые свойства Плотность: 7.83 г/см3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |