EI481-Sh (4Х12Н8Г8МФБ-Ш)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-1213-75 |
63.13–70.65 |
0.3–0.7 |
7.5–9.5 |
11.5–13.5 |
< 0.12 |
< 0.2 |
7–9 |
1.25–1.55 |
< 0.035 |
0.35–0.4 |
< 0.015 |
0.35–0.45 |
1.1–1.4 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Berechnete Eigenschaften Dichte: 7,79 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |