EI554
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Mo, % | N, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 70.65–75.85 | < 0.4 | < 0.4 | 3.8–4.6 | < 0.4 | 1–1.4 | 1–1.5 | < 0.03 | 0.8–0.9 | < 0.02 | < 0.5 | 0.05–0.2 | 17.5–19 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 9.78 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
| W | % | Tungsten |