EI566
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 89.86–92.67 | < 0.35 | 0.2–0.4 | 2.5–3 | 0.08–0.15 | < 0.25 | 0.2–0.5 | < 0.03 | 0.35–0.43 | < 0.03 | 4–5 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 8.32 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |