EI59

Classification

Country Section Category
CIS, Russia, Ukraine Corrosion-resistant alloys and steels Corrosion-resistant heat-resistant steel

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ni, % P, % C, % S, %
60.24–73 < 1.2 < 0.7 27–37 < 0.6 < 0.03 < 0.2 < 0.03

Information on suppliers

Свойства

Свойство
Вычисляемые свойства Плотность: 7.6 г/см3

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Ni % Nickel
P % Phosphorus
C % Carbon
S % Sulfur