EI639 (67Н26М, NIMO-25)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-1144-74 |
2.175–9 |
< 0.25 |
< 0.5 |
62.175–72.825 |
< 0.02 |
< 0.035 |
< 0.02 |
25–28 |