EI643-VD (40HN2SMA-VD)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-3-674-78 |
94.18–95.54 |
0.9–1.2 |
0.25–0.5 |
0.8–1.1 |
1.8–2.1 |
< 0.025 |
0.36–0.44 |
< 0.005 |
0.35–0.45 |
Information on suppliers
Properties
| Property |
| Calculated Properties Density: 7.81 g / cm3 |