EI657 (X28AN)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|---|---|
| 67.34–73.82 | < 1 | < 1.5 | 25–28 | 1–1.7 | < 0.035 | < 0.15 | < 0.025 | 0.18–0.25 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.63 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |