EI692 (HN35VMT)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % | N, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 38.71–48.6 | < 0.6 | < 1 | 14–16 | 1.1–1.5 | 32–36 | < 0.03 | < 0.12 | < 0.02 | 2–3 | < 0.02 | 2.3–3 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 8.41 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
| W | % | Tungsten |