EI694P (1X14N16BR)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ni, % | Ce, % | P, % | C, % | S, % | Nb, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 63.9–71.03 | < 0.6 | < 0.005 | 1–2 | 13–15 | 14–17 | < 0.02 | < 0.035 | 0.07–0.12 | < 0.02 | 0.9–1.3 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.91 g / cm3 |