EI696M
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
| GOST 14162-1979 |
48.32–51 |
< 0.3 |
0.3–0.6 |
0.7–1 |
< 0.2 |
48–49.5 |
< 0.015 |
< 0.05 |
< 0.015 |
Information on suppliers
Properties
| Property |
| OST blanks 108.961.05-80 Application temperature: <650 ° C |
| Billets according to OST 108.961.05-80 Discs KP75 Strength Category Tensile Strength:> 1079 MPa Elongation:> 14% Elongation:> 15% Yield:> 736 MPa |
| Calculated Properties Density: 7.9 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |