EI712M (EP506)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-1-1122-74 |
92.28–94.51 |
0.17–0.37 |
0.6–0.9 |
1.9–2.4 |
1.2–1.6 |
0.18–0.28 |
< 0.03 |
0.09–0.16 |
< 0.03 |
0.35–0.55 |
1–1.4 |
Information on suppliers
Properties
| Property |
| Calculated properties Density: 7.99 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |