EI733
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|
| 88.285–90.95 | 1.5–2 | 1.7–2.2 | 3.25–3.75 | 1.5–2 | < 0.03 | 0.35–0.45 | < 0.035 | 0.75–1.25 |
Information on suppliers
Properties
| Property |
|---|
| Calculated Properties Density: 7.85 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |