EI778
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 11.95–22.495 | < 0.5 | 0.005–0.01 | 1–1.5 | 15–18 | 1.5–1.9 | 49.455–65.545 | < 0.02 | < 0.1 | < 0.02 | 5–6 |
Information on suppliers
Properties
| Property |
|---|
| Calculated properties Density: 8.9 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |