EK116
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 2 | < 0.3 | < 0.01 | < 0.03 | < 0.4 | 5.5–10 | 12–14.5 | 0.6–1.4 | < 0.07 | 55.88–70.08 | 0.7–1.2 | < 0.005 | 2.1–2.6 | < 0.01 | < 0.015 | 0.02–0.06 | < 0.01 | 2.8–3.3 | < 0.01 | 3.6–4.6 | 2.6–3.6 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| La | % | Lanthanum |
| Mo | % | Molybdenum |
| W | % | Tungsten |