EK145
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 30.887–38.6 | < 0.3 | 6–7.5 | < 0.05 | 14–16 | < 0.3 | 34–36 | < 0.1 | < 0.018 | < 0.03 | < 0.015 | 1.4–1.8 | 6–7 |