Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
Zr, % |
Al, % |
Ce, % |
P, % |
C, % |
Nb, % |
La, % |
Mo, % |
Tl, % |
| TU 14-1-1213-75 |
12–16 |
< 0.5 |
< 0.7 |
14.5–18.5 |
0.2–1 |
0.1–1 |
49.77–65.4 |
0.3–0.6 |
< 0.02 |
0.5–1.3 |
< 0.02 |
< 0.015 |
< 0.05 |
4–5.5 |
< 0.01 |
3–5 |
< 0.015 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| Nb |
% |
Niobium |
| La |
% |
Lanthanum |
| Mo |
% |
Molybdenum |
| Tl |
% |
Thallium |