EN AC-21100
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
OE, % |
ET, % |
| EN 12392:2016 |
< 0.19 |
< 0.18 |
< 0.55 |
0.15–0.3 |
4.2–5.2 |
< 0.07 |
93.45–95.65 |
< 0.03 |
< 0.03 |