EP235
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 24.73–33.7 | < 0.35 | 7–8.5 | 14–16 | 1.3–1.8 | 27.03–42.97 | < 0.02 | < 0.08 | < 0.02 | 3–4 | 7–8.5 |