EP741NP (HN51KVMTYUB)
for the manufacture of heat-resistant articles critical applications
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Granulated nickel superalloy Alloy |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | Pb, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 52802-2007 | < 2 | < 0.5 | 0.011–0.013 | < 0.4 | 13–16 | 2.35–2.75 | 71.034–78.559 | 1.45–1.8 | < 0.001 | < 0.01 | < 0.015 | 0.03–0.07 | < 0.007 | 1.8–2.2 | 2.8–3.2 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 52802-2007 | GOST |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |