EP743 (00H20N42M4V3B)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 20.825–31.1 | < 0.5 | 1.2–1.8 | 20–22 | 34.725–50.275 | < 0.02 | < 0.04 | < 0.015 | 0.9–1.3 | 4–5 | 2.8–3.5 |