EP753-DID (02H18N40M5G2TFRYU-IDD)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
| TU 14-159-264-97 |
32–37.7 |
< 0.1 |
1–2 |
17.5–19 |
35.3–44.7 |
0.05–0.2 |
< 0.05 |
< 0.01 |
< 0.01 |
< 0.015 |
0.25–0.6 |
4.5–5 |
< 0.015 |