EP753RTYU (HN40MGBTYUR)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 27.243–36.299 | < 0.2 | 0.001–0.007 | 1–2 | < 0.01 | 17.5–19.5 | 0.9–1.5 | 32.944–48.056 | 0.05–0.2 | 0.5–0.9 | < 0.15 | < 0.01 | < 0.02 | < 0.01 | 0.25–0.6 | 4.5–5.5 | < 0.15 |