EP754-ID (015H20N25G2B-ID)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
N, % |
| TU 14-1-3276-81 |
49.45–52.85 |
< 0.1 |
1.5–2.2 |
20–21 |
25–26 |
0.05–0.3 |
< 0.01 |
< 0.015 |
< 0.01 |
0.6–0.9 |
< 0.015 |