EP864 (03H21N32M3B)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
| TU 14-1-2511-78 |
37.605–44.6 |
< 0.8 |
< 1 |
20–22 |
< 0.1 |
< 0.2 |
31.5–33 |
< 0.02 |
< 0.03 |
< 0.015 |
0.9–1.2 |
3–4 |
< 0.03 |