ERH 99.97-MP
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Cr, % | Cu, % | Ni, % | Al, % | C, % | S, % | O, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|
| < 0.01 | < 0.002 | > 99.959 | < 0.002 | < 0.001 | < 0.002 | < 0.007 | < 0.002 | < 0.01 | < 0.005 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| S | % | Sulfur |
| O | % | Oxygen |
| N | % | Nitrogen |