ET2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Wrought Titanium Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Al, % | C, % | O, % | N, % | H, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|
| < 0.2 | < 0.1 | 96.275–97.6 | 2.4–2.9 | < 0.08 | < 0.1 | < 0.03 | < 0.015 | < 0.3 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Al | % | Aluminium |
| C | % | Carbon |
| O | % | Oxygen |
| N | % | Nitrogen |
| H | % | Hydrogen |