FA65
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Cu, % |
Al, % |
Pb, % |
P, % |
C, % |
S, % |
Примеси, % |
| TU 14-2Р-381-2004 |
10.58–38 |
< 4 |
< 0.3 |
< 3 |
< 2.5 |
40.58–89.42 |
< 0.3 |
< 0.06 |
< 0.7 |
< 0.06 |
< 10.5 |