FeMn90C01
Low carbon ferromanganese.
In the steel and foundry industry for the alloying of steel and its deoxidation
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | ferromanganese |
Chemical composition
| Standard | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|
| GOST 4755-91 | < 2 | 85–95 | < 0.3 | < 0.1 | < 0.03 |