FeSi45
It is used in steel making and foundry industry for deoxidization and as an alloying element in the production of corrosion-and heat-resistant, electrical and spring-spring steels.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | ferrosilicium |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ti, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1415-93 | 41–47 | < 1 | < 0.5 | < 0.3 | < 2 | < 0.05 | < 0.2 | < 0.05 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1415-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |