FeT40A18
It is used in steel making and foundry industry for deoxidation and alloying of steel and alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | ferrotitanium |
Chemical composition
| Standard | Si, % | Mn, % | Ti, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 4761-91 | < 5 | < 1.5 | 35–50 | < 8 | < 0.05 | < 0.1 | < 0.05 |