FHP850A
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % | P, % |
|---|---|---|---|
| 34.96–35 | 64.96–65.04 | < 0.04 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |
| P | % | Phosphorus |