FMo50
It is used in steel making and foundry industry as an alloying element to give a homogeneous fine-grained structure steel; improves hardenability and hardenability of steel, increases its viscosity, eliminate temper brittleness of chromium-nickel steel, it contributes to the preservation properties of steel at high temperatures; ferromolybdenum in iron supplement increases its durability and wear resistance.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | ferro |
Chemical composition
| Standard | Si, % | Sn, % | Cu, % | Sb, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|
| GOST 4759-91 | < 3 | < 0.1 | < 2 | < 0.1 | < 0.1 | < 0.5 | < 0.5 | > 50 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 4759-91 | |
| DSTU GOST 4759:2009 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Sn | % | Tin |
| Cu | % | Copper |
| Sb | % | Antimony |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |