Fn-3
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
| TU 48-3-59-84 |
82.95–85 |
< 0.1 |
< 0.05 |
< 0.35 |
< 0.5 |
< 0.5 |
> 15 |
< 0.05 |
< 0.2 |
< 0.1 |
< 0.2 |
Note: Ni: Ni + Co
Note: W + Mo <0.5