FNb15S15
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Al, % | P, % | S, % | Nb, % |
|---|---|---|---|---|---|---|---|
| TU 14-141-28-94 | 51.42–74 | 10–20 | < 3 | 1–5 | < 0.5 | < 0.08 | 15–20 |
Note: Nb: Nb + Ta
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-141-28-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Al | % | Aluminium |
| P | % | Phosphorus |
| S | % | Sulfur |
| Nb | % | Niobium |