FNb60
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ti, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Ta, % |
| GOST 16773-2003 |
28.27–45 |
< 1.5 |
< 1 |
< 3 |
< 0.1 |
< 0.1 |
< 0.03 |
48.27–71.73 |
< 1 |