Fng
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Mn, % | Co, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 86.22–90 | < 0.05 | < 0.5 | < 1 | < 0.5 | > 10 | < 0.03 | < 0.35 | < 0.35 | < 0.5 | < 0.5 |
Note: Ni: Ni + Co
Note: Si, Al, Mn - not limited